MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Copper Alloy, UNS C66950, H02 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard

Fabrication Properties: Good Suitability – Gas Shielded Arc Welding, Spot Weld, Butt Weld

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 95
@Load 0.500 kg
95
@Load 1.10 lb
Tensile Strength 448 MPa65000 psi
Tensile Strength, Yield 200 MPa29000 psi0.2% Offset
Elongation at Break 35 %35 %
Tensile Modulus 125 GPa18100 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000510 ohm-cm0.0000510 ohm-cm3.4% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 22.5 µm/m-°C
@Temperature 20.0 - 300 °C
12.5 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 2.88 W/m-K20.0 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.0 - 1.5 %1.0 - 1.5 %
Copper, Cu 68 - 71 %68 - 71 %As Balance
Iron, Fe <= 0.50 %<= 0.50 %
Lead, Pb <= 0.010 %<= 0.010 %
Manganese, Mn 14 - 15 %14 - 15 %
Zinc, Zn 14 - 15 %14 - 15 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC66950x1 / 292333

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.