MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller Körapur 940 Marine Adhesive and sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Elastic, one component moisture curing adhesive and sealant suitable for use in the marine and boat industry:
  • Good adhesion to primed and painted metals, aluminum, wood and duroplastics, GRP and gel coat
  • Deck-to-hull bonding
  • Construction adhesive
  • Good resistance to humidity and weathering
  • Resistant to temperatures from –40°C to +90°C (for short intervals up to +120°C)
  • High resistance to sagging
  • Fast curing
  • Overpaintable after curing
  • Spreadable
  • Meets the requirements of the International Maritime Organization

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
Storage Temperature <= 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55DIN 53 505
Tensile Strength 4.00 MPaDIN 53 504
Elongation at Break 400 %DIN 53 504
Shear Strength 3.00 MPa
@Thickness 2.00 mm
Lap; DIN 53283
Tear Strength 7.00 kN/mDIN 53 515
 
Processing PropertiesOriginal ValueComments
Cure Time 70.0 - 90.0 minSkin formation time
Shelf Life 6.00 MonthDrums
 9.00 MonthSachets
 9.00 MonthCartridges
 
Descriptive Properties
Base compoundPolyurethane, one-component, cures on exposure to humidity
ColorWhite, grey, black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL138 / 316929

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.