MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger HYDEX® 4101 PBT black Polybutylene terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes:
  • resistant to cleaning agents
  • very good chemical resistance
  • good wear resistance
  • good impact strength
  • low moisture absorption
Target Industries:
  • gear manufacturing
  • mechanical engineering
  • chemical plant engineering
  • packaging and paper machinery
  • conveyor technology
  • semiconductor technology
  • clean room technology
  • automotive industry

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³
Moisture Absorption 0.0200 %
@Time 86400 sec
0.0200 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8787ASTM D 785
Tensile Strength, Yield 64.8 MPa9400 psiASTM D 638
Elongation at Break 50 %50 %ASTM D 638
Elongation at Yield 6.0 %6.0 %ASTM D 638
Modulus of Elasticity 2.96 GPa430 ksiASTM D 638
Flexural Strength 89.6 MPa13000 psiASTM D 790
Flexural Modulus 2.96 GPa430 ksiASTM D 790
Compressive Yield Strength 79.3 MPa
@Strain 10 %
11500 psi
@Strain 10 %
ASTM D 695
Compressive Strength 19.3 MPa
@Strain 1 %
2800 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 2.17 GPa315 ksiASTM D 695
Izod Impact, Unnotched 0.374 J/cm0.700 ft-lb/inASTM D 256
Coefficient of Friction, Dynamic 0.25
@Pressure 0.276 MPa
0.25
@Pressure 40.0 psi
50 fpm
Coefficient of Friction, Static 0.190.19
K (wear) Factor 423 x 10-8 mm³/N-M210 x 10-10 in³-min/ft-lb-hr2000 PV
Limiting Pressure Velocity 0.210 MPa-m/sec6000 psi-ft/min@ 100 fpm, per LNP EPALP-TB003
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C61.0 µin/in-°F
Maximum Service Temperature, Air 105 °C221 °FLong Term
Deflection Temperature at 0.46 MPa (66 psi) 154 °C310 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C200 °FASTM D 648
Flammability, UL94 HBHB
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8140 / 319068

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.