MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ixom PROTEQ™ H10T4 PP, 20% Talc Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: PROTEQ™ H10T4 is a medium flow 20% Talc filled grade of polypropylene homopolymer.

Information provided by Ixom Operations PTY LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78instantaneous; ISO 868
 73
@Time 15.0 sec
ISO 868
Tensile Strength 31.0 MPa12.7 mm x 3.2 mm @ 5.0 mm/min; ASTM D638
Elongation at Break 30 %12.7 mm x 3.2 mm @ 5.0 mm/min; ASTM D638
Flexural Strength 48.0 MPa12.7 mm x 3.2 mm @ 1.3 mm/min; ASTM D790
Flexural Modulus 2100 MPa12.7 mm x 3.2 mm @ 1.3 mm/min; ASTM D790
Izod Impact, Notched 40.0 J/m12.7 mm x 3.2 mm; ASTM D256
Izod Impact, Unnotched 395 J/m12.7 mm x 3.2 mm; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 135 °C12.7 mm x 3.2 mm; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C12.7 mm x 3.2 mm; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
Glow Wire Ignition Temperature 550 °C
@Thickness 1.60 mm
AS/NZS 60695
Shrinkage 1.2 %3.0 mm plaque; ASTM D955
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 195 - 215 °C
Middle Barrel Temperature 205 - 225 °C
Front Barrel Temperature 215 - 235 °C
Melt Temperature 220 - 270 °C
Mold Temperature 50.0 - 80.0 °C
Drying Temperature 85.0 - 90.0 °CTemperature of pellet bed
Dry Time 2.00 - 4.00 hourat desired pellet bed
Injection Pressure 60.0 - 140 MPa
Back Pressure 0.100 - 0.500 MPa
Screw Speed 40 - 60 rpm
 
Descriptive Properties
Clamp pressure3 - 6 kN/cm²

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PIXOM019 / 283100

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.