MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical LUCENE™ LF775 Polyolefin Elastomer
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Applications:
  • General purpose thermoplastic elastomer for polymer modification
  • Photovoltaic encapsulant
Typical properties:
  • LUCENETM LF775 is an ethylene-1-butene copolymer produced using LG Chem's metallocene polymerization catalyst and solution process technology.
  • LUCENETM LF775 is an excellent impact modifier for plastics and offers unique performance capabilities for compounded products.
  • LUCENETM LF775 contains antioxidants only.

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.878 g/ccASTM D1505
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75ASTM D2240
Tensile Strength at Break 6.40 MPa500 mm/min; ASTM D638
Elongation at Break >= 1000 %500 mm/min; ASTM D638
Flexural Modulus, 1% Secant 20.0 MPaASTM D790
Tear Strength 31.6 kg(f)/cmASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 65.0 °C
Glass Transition Temp, Tg -47.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUCENE™ LC875 Polyolefin Elastomer
LG Chemical LUCENE™ LC168 Polyolefin Elastomer
LG Chemical LUCENE™ LC100 Polyolefin Elastomer
LG Chemical LUCENE™ LC160 Polyolefin Elastomer
LG Chemical LUCENE™ LC161 Polyolefin Elastomer

PLHCHEM9870 / 239386

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.