MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX GTX989 PPE+PA (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted body panels and fenders in particular. This material combines impact performance with conductivity for electro-static painting in an unique way.

Information provided by SABIC Innovative Plastics for the Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D 792
Density 1.08 g/ccISO 1183
Moisture Absorption 1.20 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 4.2 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.012 - 0.016 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D 1238
 19 g/10 min
@Load 5.00 kg,
Temperature 280 °C
cm^3/10 min Melt Volume Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPa50 mm/min; ISO 527
 60.0 MPaType I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527
 65.0 MPaType I, 50 mm/min; ASTM D 638
Elongation at Break 40 %50 mm/min; ISO 527
 45 %Type I, 50 mm/min; ASTM D 638
Elongation at Yield 5.0 %50 mm/min; ISO 527
 5.0 %Type I, 50 mm/min; ASTM D 638
Tensile Modulus 2300 MPa1 mm/min; ISO 527
 2350 MPa50 mm/min; ASTM D 638
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 95.0 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2300 MPa2 mm/min; ISO 178
 2450 MPa1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 180 J/m
@Temperature -30.0 °C
ASTM D 256
 240 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 22.0 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -30.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 22.0 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 60.0 J
@Temperature 23.0 °C
ASTM D 3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 - 10000 ohm-cmSABIC Method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 85.0 µm/m-°C
@Temperature -40.0 - 60.0 °C
ASTM E 831
 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 85.0 µm/m-°C
@Temperature -40.0 - 60.0 °C
ASTM E 831
 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 190 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 190 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Vicat Softening Point 195 °CRate B/50; ASTM D 1525
 195 °CRate B/50; ISO 306
 200 °CRate B/120; ISO 306

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® T95 MF Polycarbonate + ABS, Mineral Filled

PSABI47357 / 188442

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.