MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ASI® FLEX 1300 Silicone Adhesive/Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: FLEX 1300 is a red, one component, high modulus, high temperature resistant, silicone adhesive sealant, which cures to a tough rubbery solid upon exposure to air. FLEX 1300 operates within a continuous temperature range of -60 to 260°C and for intermittent periods up to 315°C.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/cc
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °Ccontinuous
 315 °Cintermittent
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
 
Descriptive Properties
Color / appearanceRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain CHR® M52 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Parker Chomerics Tecknit® 0236 Conductive Silicone Sealant/Adhesive
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
NuSil R-2180 Silicone Engineering Coating
NuSil CF1-6755 Silicone Two Part Sealing & Adhesive

PASINC9220 / 233586

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.