MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

RAMPF RAKU® TOOL PH-3978 Polyurethane Adhesive
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Two component, unfilled polyurethane, can be filled with AC-9004

Key Properties:

  • Unfilled, very low viscosity
  • High fill rate possible
  • Good cure
  • Very high strength
  • Good temperature resistance
Applications:
  • Foundry patterns, core boxes, negatives, pattern plates
  • Checking casts
  • Replicas
  • Vacuum forming molds
  • Jigs
Cure: 7 days at RT or 14h at 104°F (40°C)

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D-792
 1.60 - 1.70 g/cc0.0578 - 0.0614 lb/in³PF-3708/PH-3978 - AC-9004, Cured; ASTM D-792
Viscosity 80 - 100 cP80 - 100 cPASTM D-2393
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 8580 - 85PF-3708/PH-3978 - AC-9004, Cured; ASTM D-2240
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 - 120 min1.00 - 2.00 hourPF-3708/PH-3978 - AC-9004, Demold time
Pot Life 5.00 - 6.00 min5.00 - 6.00 minPF-3708/PH-3978 - AC-9004; ASTM D-2393
 
Descriptive Properties
AspectWhitePF-3708/PH-3978 - AC-9004, Cured
ColorLight yellow
Mix Ratio100Weight
 86Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF008 / 317608

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.