MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxygen-free extra-low phosphorus Copper, UNS C10300, H04 Temper, Shapes
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Butt Weld; Fair Suitability – Oxyacetylene Welding

Common Fabrication Processes: Blanking, Coining, Coppersmithing, Drawing, Etching, Forming and Bending, Heading and Upsetting, Hot Forging and Pressing, Piercing and Punching, Roll Threading and Knurling, Shearing, Spinning, Squeezing and Swaging, Stamping

Typical uses: Applications Requiring High Conductivity; Busbars; Clad Products; Commutators; Electrical Conductors; Terminals; Thermostatic Control Tubing; Tubular Bus; Wave Guide Tubing; Applications Requiring Good Brazing; Applications Requiring Good Weldability; Billet Mold Tube; Extrusion Cans for Powder Metallurgy; Pressure Vessels

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 3535
Tensile Strength 276 MPa40000 psi
Tensile Strength, Yield 221 MPa32000 psi
Elongation at Break 30 %30 %
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Machinability 20 %20 %
Forgeability 65 %65 %
Shear Strength 179 MPa26000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000174 ohm-cm0.00000174 ohm-cm99% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.9 µm/m-°C
@Temperature 20.0 - 100 °C
9.40 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.60 µin/in-°F
@Temperature 68.0 - 392 °F
 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 32.1 W/m-K223 BTU-in/hr-ft²-°F
Melting Point 1083 °C1981 °F
Annealing Point 371 - 649 °C700 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 760 - 871 °C1400 - 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.95 %>= 99.95 %
Lead, Pb 0.0010 - 0.0050 %0.0010 - 0.0050 %
 
Descriptive Properties
Cold Work (%)15
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC10300x3 / 292660

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.