MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue Stick
Categories: Polymer; Adhesive; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue Stick
Medium performance. Oil resistance for wood, fabric and other porous substrates primarily in woodworking assembly operation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 11500 cP
@Temperature 177 °C
11500 cP
@Temperature 350 °F
Typical
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 91.1 °C196 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 0.083 - 0.50 min0.083 - 0.50 minOpen Time
 
Descriptive Properties
ColorClear Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Valley Adhesives EM-422 High Temperature Application Glue Stick
Parson Adhesives PARLITE® 4760 UV Glue and UV Adhesive for Electronic Assembly
Lord Adhesives 360 Sag-Resistant, High-Performance, 5 min Epoxy Adhesive
Chemical Concepts H2O Glue® Aquabonder Underwater Adhesive
Bostik 6332 Quick Setup EVA Glue Stick

PBOST05 / 27564

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.