MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® Perfluor GA-500 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® Perfluor GA-500 is a perfluoroelastomer with outstanding heat resistance and chemical resistance compared with other fluoroelastomers and can be used under severe conditions. Perfluor GA-500 is also suitable for semiconductor applications due to its high level of cleanliness.

Typical Applications: Hydrocarbons, fuels, ketones, halogenated hydrocarbons, esters, alkalis and amines, ethers, mineral and organic acids, alcohols, steam

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.00 g/cc
Mooney Viscosity 80
@Temperature 100 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74
Tensile Strength at Break 19.0 MPa
Elongation at Break 200 %
100% Modulus 8.00 MPa
@Strain 100 %
Compression Set 15 %
@Temperature 3000 °C,
Time 252000 sec
P-24 O-ring, 25% deformation, 30 min recovery
 31 %
@Temperature 316 °C,
Time 252000 sec
P-24 O-ring, 25% deformation, 30 min recovery
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °Ccontinuous use
 320 °Cpeak for short time
 
Processing PropertiesOriginal ValueComments
Cure Time 14.1 min(JRS Type II: 10 mins @160°C), T90
 15.0 min
@Temperature 180 °C
Press Cure
 18.0 hour
@Temperature 290 °C
Post cure
 
Descriptive Properties
ColorWhite or transparent sheet
Detection limit0.5 ppmFe
 0.5 ppmCr
 0.5 ppmNi
 0.5 ppmNa
 0.5 ppmK
 0.5 ppmCa
 0.5 ppmMg
 0.5 ppmCu
 0.5 ppmZn
 1.0 ppmAl
Test Formula0.8 phrVulcanizing agent V-6M
 100 phrBase Polymer
 20 phrCarbon black MT (N-990)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin DAI-EL® G-952 Fluoroelastomer Terpolymer, 69% Fluorine Content

PDAIJ9871 / 209942

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.