Product Description: HD035-GP is designed for applications requiring excellent stiffness and stress crack resistant properties. It may be used as a sheet extrusion thermoforming resin or a general purpose blow molding resin. Suggested uses would include bottles and containers for bleach and detergents, personal care products and pharmaceutical packaging Availability: Africa & Middle East; Asia Pacific; Europe; Latin America Features: Copolymer: High Density; High ESCR (Stress Crack Resist.); High Stiffness Uses: Automotive Applications; Bottles; Containers; Packaging; Pharmaceutical Packaging Processing Method: Blow Molding; Sheet Extrusion; Thermoforming Information provided by Osterman & Company |