MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Diofan® A 736 Polyvinylidene Chloride (PVDC)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyvinyl Dichloride (PVDC)

Material Notes: DIOFAN® A 736 is a PVDC water-based dispersion recommended for use as a flexible underlayer for barrier coating on rigid PVC or PVC/ PE film, to be covered with DIOFAN® 193 D as top coat. The film structure is used for blister application in pharmaceutical packaging.

Key Attributes: Good Flexibility; Moisture Barrier; Oxygen Barrier

Applications: Barrier Coatings; Coating Applications

Agency Ratings: DMF 11383; EC 1907/2006 (REACH); EU No 10/2011; FDA 21 CFR 175.300; FDA 21 CFR 175.320; FDA 21 CFR 176.170; FDA 21 CFR 176.180

DELIVERY AND STORAGE
- Diofan® A 736 is delivered in bulk or in Intermediate Bulk Containers (IBC). Bulk supplied latex should be stored in reservoirs made of suitable stainless steel, HDPE, rigid PVC or glass fiber-reinforced polyester.
- Contact of anionic Diofan® dispersion with metals like iron, zinc, aluminum and copper as well as alloys such as brass and bronze must be avoided.
- Keep the vessels tightly closed to prevent drying through evaporation. Store the product ideally between 5°C and 25°C (41 °F and 77°F) to avoid degradation.
- IBC should be protected from sunlight exposure.

PROCESSING - DRYING
- Diofan® A 736 can be processed with different coating techniques, including reverse gravure roll and air knife coating systems.
- Diofan® coatings require adequate drying conditions, since, in general, higher temperatures will result in better barrier properties.ISO CERTIFICATION
- The implemented management system for the production, internal transfer and delivery, design and development of Diofan® vinylidene chloride copolymers (PVDC) produced in Tavaux has been assessed and found to meet the requirements of ISO 9001: 2008, ISO 14001: 2004 and OHSAS 18001: 2007.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 18.0 g/m²/day
@Thickness 0.00100 mm,
Temperature 38.0 °C
90% RH; ASTM F1249
Oxygen Transmission Rate 21.0 cc/m²/day
@Thickness 0.00100 mm,
Temperature 23.0 °C
85% RH; ASTM D3985
 
Mechanical PropertiesOriginal ValueComments
Tensile Impact Strength 500 kJ/m²ASTM D1822
 
Descriptive Properties
Availability (as of March 2019)Asia Pacific; Europe; Latin America; North America
ColorMilky White
FormsLiquid

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y5132 / 238513

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.