Key Features: - Long open time at room temperature
- Cures at moderately elevated temperatures
- Superb physical strength profile
- Passes ISO 10993-5
Product Description: Master Bond EP62-1HTMed is a two component epoxy system with a long working life at ambient temperature. The mix ratio is a forgiving 100 to 5 by weight. Upon mixing, it is a moderate viscosity system that flows well. The working life of 100 grams is 12-24 hours at room temperature. The cure schedule options are as follows, 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C]. However to obtain optimum properties, post curing at 212-302°F [100-150°C] for 3-5 hours is strongly recommended. The epoxy contains no solvents or diluents and has low shrinkage upon cure. The system bonds well to a wide variety of substrates such as metals, plastics, rubbers, ceramics and composites. Upon curing with the optimum schedule, EP62-1HTMed excels in combining high temperature resistance along with the ability to withstand repeated sterilization and many aggressive chemicals. It has a high glass transition temperature (see below). EP62-1HTMed is a dependable electrical insulating material. The service temperature range is -60°F to +450°F. The color of Part A is clear and Part B is dark brown. It is especially well suited for applications where harsh sterilants are being employed. Product Advantages: - Very long working life
- Good flow properties
- Versatile curing schedules
- Highly resistant to chemicals
- Withstands repeated sterilization including autoclaving
Information provided by Master Bond. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |