MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC 430BE LLDPE (Global)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: SABIC® LLDPE 430BE is a butene linear low density polyethylene resin. The material, natural resin, is typically used for cast film applications, offering good mechanically properties, stiffness enhancement and furthermore enables to gain high line speeds. SABIC® LLDPE 430BE is provided with a dedicated anti oxidant package suitable for cast film extrusion with low gel levels. Applications Skin layers for non-cling stretch cast film, cast film side encapsulation, mid layer hygienic cast film and product to realize downgauging by stiffness enhancement. Film properties Properties are determined on 20 µm cast stretch film produced on a 2 m commercial cast stretch line: melt temperature 270 °C, chill roll temperature 20 °C and line speed of 450 m/min. Processing conditions SABIC® LLDPE 430BE is extrudable with conventional cast film extrusion equipment. Minor machine modifications may be required for optimum use. Cast film melt temperatures 250 - 300 °C. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by Sabic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D1505
Melt Flow 4.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Puncture Energy 0.500 JASTM D5748-95
Tear Strength 117 kN/mTD; ISO 6383-2
Dart Drop Total Energy 15.0 J/cmISO 7765-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 124 °CSABIC method
Vicat Softening Point 109 °Cat 10 N (VST/A); ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 2.4 %ASTM D1003
Gloss 91 %at 45°; ASTM D2457
 
Descriptive Properties
Elastic recovery & Stress retention45 %ASTM D5459-95; Elastic recovery
 78 %ASTM D5459-95; Stress retention

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI32228 / 229737

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.