MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Biowert AgriPlast NFLDPE 3070/40000 HM Grass Fibre-Reinforced Thermoplastics for Injection Moulding and Extrusion
Categories: Polymer; Thermoplastic

Material Notes:
  • AgriPlast NFLDPE 3070/40000 HM Is made up of 30% cellulose fibres obtained from meadow grass and 70% low density polyethylene.
  • AgriPlast BW granules can be used with any injection moulding machine and processed into moulded components such as spoons, consoles, machine cases, protective caps, etc. The granules can also be dyed any colour.
  • Ideal ease of flow for injection moulding. High cycle times when manufacturing complex moulded parts.
  • AgriPlast BW is lighter than comparable fibre-reinforced composite plastics.
  • Fire protection without antimony and halogen.
  • Recyclable and residue-free disposal when incinerated.
  • Processing notes For AgriPlast NFLDPE 3070/40000 HM: Sufficiently dry at 70 – 80 °C, heating zones of 200 °C Decreasing to 170 °C, possible short-term peak melting temperature of 210 °C, moulding temperature of 40 – 50 °C, avoid frictional and shearing heat, make sure the tool is well ventilated.

Information provided by Biowert Industrie GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.014 g/cc0.03663 lb/in³DIN EN ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 12.2 MPa1770 psiDIN EN ISO 527
Tensile Strength, Yield 12.2 MPa1770 psiDIN EN ISO 527
Elongation at Break 4.94 %4.94 %Tensile Strength; DIN EN ISO 527
Elongation at Yield 4.93 %4.93 %DIN EN ISO 527
Tensile Modulus 0.542 GPa78.6 ksiDIN EN ISO 527
Flexural Strength 16.1 MPa2340 psiDIN EN ISO 178
Flexural Modulus 0.515 GPa74.7 ksiDIN EN ISO 178
Flexural Strain at Break 5.1 %5.1 %Bending Strength; DIN EN ISO 178
Charpy Impact Unnotched 2.76 J/cm²13.1 ft-lb/in²DIN EN ISO 179
Charpy Impact, Notched 1.18 J/cm²5.61 ft-lb/in²DIN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 108 °C226 °FDIN EN ISO 306 B/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBIOWRT004 / 255709

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.