MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ 2210EPR PEI (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 20% Glass Fiber

Material Notes: 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 13 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 137 MPaType I, 5 mm/min; ASTM D638
Tensile Strength, Yield 137 MPaType I, 5 mm/min; ASTM D638
Elongation at Break 3.0 %Type I, 5 mm/min; ASTM D638
Elongation at Yield 3.0 %Type I, 5 mm/min; ASTM D638
Flexural Strength 206 MPa2.6 mm/min, 100 mm span; ASTM D790
Flexural Yield Strength 206 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6890 MPa1.3 mm/min, 50 mm span; ASTM D790
 6890 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 80.0 J/mASTM D256
Izod Impact, Unnotched 587 J/mASTM D4812
Instrumented Impact Total Energy 14.0 JASTM D3763
Tangent Modulus 6890 MPa5 mm/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 60 - 120 secUL 746A
High Amp Arc Ignition, HAI 15 - 30 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 36.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 211 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 213 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 208 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 210 °CRate B/50; ASTM D1525
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 V-0
@Thickness 0.400 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 400 °C
Zone 1 330 - 400 °C
Zone 2 340 - 400 °C
Zone 3 345 - 400 °C
Melt Temperature 350 - 400 °C
Mold Temperature 135 - 165 °C
Drying Temperature 150 °C
Dry Time 4.00 - 6.00 hour
 24.0 hourCumulative
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI22553 / 215689

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.