MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Proteus® Black UV Copolymer Polypropylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Please note: This data is preliminary and is subject to change as further data is gathered.

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccASTM D792
Water Absorption <= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %Immersion; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 73ASTM D2240
Tensile Strength 3090 psiASTM D638
Tensile Strength at 65°C (150°F) 400 psiASTM D638
Elongation at Break 265 %ASTM D638
Tensile Modulus 85.0 ksiASTM D638
Flexural Strength 5250 psiASTM D790
Flexural Modulus 137 ksiASTM D790
Compressive Strength 3800 psi10% Def.; ASTM D695
Compressive Modulus 125000 psiASTM D695
Izod Impact, Notched NBASTM D256 Type A
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+14 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Melting Point 305 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 180 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 190 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Estimated Rating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SMP66s_copy / 255384

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.