MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones SilPruf LM SCS2700 Silicone Weatherproofing Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: SCS2700 SilPruf LM silicone weatherproofing sealant is a one-component, low-modulus, neutral cure silicone for use on a wide variety of materials in new or remedial weatherproofing applications. SCS2700 is supplied as a paste and upon cure produces a durable, formed-in-place silicone rubber joint.

Features: Silicone Durability, Low Modulus, +100/-50% movement capability, Versatility with GE sealant products, Low VOC Content. Application: Adhesion, Long Tooling Time, Stable Consistency (uncured state), Low Sag or Slump.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/cc
Volatile Organic Compounds (VOC) Content 27 g/lUncured; WPSTM C1454
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 15
Tensile Strength, Ultimate 0.300 MPaC1135 specimen; hourglass shape; ATSM C1135
 1.70 MPaASTM D412
Tensile Stress at Strain 0.0600 MPa
@Strain 50 %
C1135 specimen; hourglass shape; ASTM C1135
 0.0800 MPa
@Strain 100 %
C1135 specimen; hourglass shape; ASTM C1135
Elongation, Ultimate 689 %C1135 specimen; hourglass shape.; ASTM C1135
 781 %ASTM D412
Tear Strength 5.95 kg(f)/cmDie B.; ASTM D624
Peel Strength 37.2 pli
@Temperature 23.9 °C,
Time 1.81e+6 sec
50%RH; ASTM C794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -55.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 72.0 - 96.0 hour1/4" deep section. 50% RH
 240 - 336 hourFull cure. Most common bead sizes.
Tack-Free Time 600 - 900 minASTM C679
Working Life 30.0 - 40.0 min
 
Descriptive Properties
AppearancePaste
ColorAluminum GraySCS2700.09
 BlackSCS2700.03
 BronzeSCS2700.97
 Dark GraySCS2700.10
 Light GraySCS2700.08
 LimestoneSCS2700.04
 Precast WhiteSCS2700.20
 WhiteSCS2700.02
Consistency / Sag0.1” max.ASTM D2202
Joint Movement Capability+100/-50%ASTM C719.
UV & Weathering ResistanceExcellentGE 20 yr study

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9928 / 265739

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.