Compound 9618 is a 60 durometer black colored fluorinated elastomer, it is formulated with Teflon to provide internal lubrication. It exhibits excellent resistance to heat, compression set, petroleum based oils, aromatic and aliphatic fuels. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 HK 610 A1-10 B37 B38 EF31 EO78; 4 HK 610 A1-11 B38 EF31 EO78; 6 HK 610 A1-10 A1-11 B38 EF31 EO88 Information provided by Pressure Seals Inc. |