MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Sandvik 430 Plate and sheet
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel

Material Notes: Sandvik 430 is a ferritic stainless steel with minimum 16% chromium. Due to its ferritic structure Sandvik 430 has a lower tensile strength, elongation and impact resistance than the austentic stainless steels. The proof strength is somewhat higher.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.79 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 450 MPa
Tensile Strength, Yield >= 205 MPa
@Strain 0.2 %
Elongation at Break >= 22 %
Modulus of Elasticity 220 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°C
@Temperature 20.0 - 200 °C
 10.5 µm/m-°C
@Temperature 20.0 - 400 °C
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 25.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.12 %
Chromium, Cr 16 - 18 %
Manganese, Mn 1.0 %
Nickel, Ni 0.75 %
Phosphorus, P 0.040 %
Silicon, Si 1.0 %
Sulfur, S 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
301 Stainless Steel
AK Steel 430 Ferritic Stainless steel
430 Stainless Steel annealed sheet
430 Stainless Steel annealed and cold drawn bar, 25 mm diameter
430 Stainless Steel annealed plate

NSANDV5158 / 199722

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.