Solef® 5130 PVDF is an ultra high viscosity grade that gives the best adhesion ideal for its usage in lithium batteries. Applications: Batteries; Binder Features: Good Adhesion; Ultra High Viscosity Intrinsic Viscosity: 0.27 - 0.37 l/g Information provided by Solvay Specialty Polymers. |