MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Danquinsa DANCOLL® 244-30F Non-crystallising polyurethane adduct
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: DANCOLL® 244-30F is a soft, non-crystallising polyurethane adduct. The low-molecular weight structure of this product was chosen for its application as a ground-coat and primer. DANCOLL® 244-30F is free from aromatic solvents and tin catalysts and meets the actual legislature.

Application: DANCOLL® 244-30F serves as a raw material component for very high-grade primer solvents which are mainly used for greasy leathers. As to porous substrates with a low inherent strength, the material strength is essentially improved by using DANCOLL® 244-30F as a primer. Due to its soft and elastic films, DANCOLL® 244-30F can be applied as an adherent surface for porous materials, such as leather, paper and textiles. In two-component systems, DANCOLL® 244-30F participates in the cross linking by adding polyisocyanate cross-linking agents. We recommend the addition of approx. 3 to 10 % of our hardeners DANCURE® 246-00 or DANCURE® 246-06.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/ccDIN 51.757
Solids Content 38 - 42 %DIN 53.189
Brookfield Viscosity 30000 - 57000 cPRVT
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 63 - 67Film
 
Thermal PropertiesOriginal ValueComments
Flash Point -12.0 °CDIN 51.755
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Aspectclear and yellowish liquid
SolventEthyl acetate, MEK, acetone
Typealiphatic, linear polyurethane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ017 / 294437

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.