Compound 19524 is a 50 durometer translucent colored high strength Silicone elastomer, it is formulated with FDA sanctioned materials. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 3 FC 510 A19 B37 EO16 F1-11 G11 EA14; 4 FC 510 A19 B37 EO16 F1-11 G11 EA14; 4 FE 512 A19 B37 EA14 EO16 EO36 F19 G11; 9 GE 512 A19 B37 EA14 EO16 EO36 F19 G11; 5 GE 509 A19 EA14 EO16 EO36 F19; 4 GE 507 A19 B37 EA14 EO16 EO36 F19; 3 GE 504 A19 B37 EA14 EO16 EO36 F19 AMS 3302 AMS 3347 Information provided by Pressure Seals Inc. |