VESTAMID® LX9017 natural color is a plasticized polyamide 12 compound with heat and light stabilizer for the extrusion of flexible tubing and hose, especially for automotive applications according to SAE J844. VESTAMID® LX9017 is distinguished by an easy processing as well as by a high impact strength at low temperatures. Properties of compounds based on PA 12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance. VESTAMID® LX9017 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Property data for dry samples. Information provided by Evonik. |