MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Huber Onyx Elite® 255 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Onyx Elite® 255 is a high purity alumina trihydrate used in the manufacture of solid surface cast polymers. Improved physical performance of solid surface materials results from the selected particle size distribution of Onyx Elite® 255. This product yields low viscosities, excellent air release, reduced matrix settling and a very homogenous casting. Onyx Elite® 255 has a broad particle distribution with a controlled top size (<5% on 100 mesh) which yields excellent packing characteristics. The median particle diameter, controlled particle distribution and low contaminant level of Onyx Elite® 255 aid manufacturers in obtaining good cure, good translucency and excellent color, when compared to other products offered for solid surface applications.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.42 g/cc
Bulk Density 1.00 g/ccloose
 1.50 g/ccpacked
Moisture Absorption 0.100 %
@Temperature 105 °C
Free
Particle Size <= 10 µm37 percent
 30 µmMedian Particle Diameter
Particle Mesh Size 100 Mesh<5% on
 200 Mesh15-20% on
 325 Mesh50% on
 325 Mesh60% through
Specific Surface Area 1.5 m²/gBET
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 0.0040 %
Loss on Ignition(%) 34.5 %
@Temperature 1000 °C
Na2O 0.020 %soluble
 0.20 %total
SiO2 0.0080 %
 
Descriptive Properties
Al(OH)3 (%)99.6
Color89 L
FunctionalityLow Viscosity Aid
Functionality: Optical effectsHigh Brightness / Transparency
Market/Application: ThermosetsSolid Surface/Cast Polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EHUBER760 / 300866

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.