MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nevicolor NEVIMID 66 A G50 NATURALE Nylon 66, 50% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Description: Polyamide 66 reinforced with 50% glass fibre

Information provided by Nevicolor

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ISO 1183
Moisture Absorption 1.50 %1.50 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/in115mm x 50mm x 3mm
Linear Mold Shrinkage, Transverse 0.0040 - 0.0050 cm/cm0.0040 - 0.0050 in/in115mm x 50mm x 3mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 205 MPa29700 psiISO 527-1/2
Elongation at Break 4.0 %4.0 %ISO 527-1/2
Modulus of Elasticity 16.0 GPa2320 ksi1 mm/min; ISO 527-1/2
Flexural Strength 315 MPa45700 psi2 mm/min; ISO 178
Flexural Modulus 14.0 GPa2030 ksiISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²8.09 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 85.0 kJ/m²40.4 ft-lb/in²ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °F120°C/h; ISO 75-1/-2
Vicat Softening Point  245 °C
@Load 5.10 kg
473 °F
@Load 11.2 lb
50°C/h; ISO 306/B
 255 °C
@Load 1.02 kg
491 °F
@Load 2.25 lb
50°C/h; ISO 306/A
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNEVI115 / 267459

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.