MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Pressure Seal 23911 Ethylene Propylene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 23911 is a 90 durometer black colored general purpose EPDM elastomer. It exhibits good resistance to automotive brake fluid, water, compression set and heat at elevated temperatures. It will remain non brittle at low temperatures. This compound is peroxide cured. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 AA 915 A13 F17 EA14; 2 BA 915 F17; 4 BA 915 A14 F17; 7 CA 915 A25 B35 F17 F18 G11 G21 EA14; 8 CA 915 A25 B35 F17 G11 G21 EA14; 6 CA 915 A25 B35 A14 F17 G11 G21

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 91
 90
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 91
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged
 92
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 92
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 92
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 92
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 92
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
Tensile Strength 1920 psi
 1820.2 psi
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged
 1826 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 1826 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 1856.64 psi
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 1866.2 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 1866.2 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
Elongation, Ultimate 135 %
 128 %
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 128 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 128 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 132 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 132 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 133 %
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged
100% Modulus 1428 psi
Tear Strength 184 pliDie C
 191 pliDie B
Compression Set 6.9 %
@Temperature 100 °C,
Time 79200 sec
Solid
 6.9 %
@Temperature 125 °C,
Time 79200 sec
Solid
 8.5 %
@Temperature 100 °C,
Time 252000 sec
Solid
 8.8 %
@Temperature 70.0 °C,
Time 79200 sec
Solid
 14.5 %
@Temperature 70.0 °C,
Time 79200 sec
Plied
 14.7 %
@Temperature 100 °C,
Time 79200 sec
Plied
 15.6 %
@Temperature 125 °C,
Time 79200 sec
Plied
 18.3 %
@Temperature 100 °C,
Time 252000 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -75.0 °F
Shrinkage 0.30 %
@Temperature 100 °C,
Time 252000 sec
Volume, Distilled water aged
 
Descriptive Properties
ColorBlack
TR-10 Temperature-46°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL237 / 318447

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.