For Laser Sintering Applications | No smoke development and excellent processing at low-temperatures Features: - Easy flowing
- No problems with material feeding
- Works on SLS and all other standard Powder Bed Fusion machines
- No Smoke Development
- Only single laser exposure
- 70% reusable
- Sharp edges possible
- High detail resolution due to small layer thicknesses
Colors: ROLASERIT is available in Natural/whiteInformation provided by Mitsubishi Chemical. |