MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lubrizol LifeSciences Carbopol® 981 NF Polymer
Categories: Polymer; Thermoplastic

Material Notes: Carbopol® 981 NF polymer meets the limits cited in the current edition of the following monographs:
  • United States Pharmacopeia/National Formulary (USP/NF) monograph for Carbomer Homopolymer Type A (Note: The previous USP/NF compendial name for this product was Carbomer 941.)
  • European Pharmacopeia (Ph. Eur.) monograph for Carbomers
  • India Pharmacopeia (IP) monograph for Carbomers
  • China Pharmacopeia (ChP) monograph for Carbomers

Information provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 1000 - 6000 cP1000 - 6000 cPRVT, 20 rpm, neutralized to pH 7.3 - 7.8, 0.2 wt% mucilage, spindle #4; Lubrizol 430-I
 4000 - 10000 cP4000 - 10000 cPRVT, 20 rpm, neutralized to pH 7.3 - 7.8, 0.5 wt% mucilage, spindle #5; Lubrizol 430-I
Ash <= 2.5 %<= 2.5 %Residue on Ignition; USP/NF
 
Descriptive Properties
AppearanceWhite, fluffy powder
Carboxylic Acid Content, Assay56-68%Lubrizol 1318-A
IdentificationPass1:200, Colorimetric test, USP/NF
 Pass1:200, Gel formation test, USP/NF
 PassInfrared spectrum, Lubrizol SA-102
 Pass1:200, Precipitate test, USP/NF
Loss on Drying<2%USP/NF
OdorSlightly acetic
Residual Monomer<2500 ppmFree acrylic acid, Lubrizol SA-005
Residual Solvent<0.3 %Ethyl acetate, Lubrizol SA-009
 <0.3 %Cyclohexane, Lubrizol SA-009

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 0299 K X 138337 E Polyarylamide (PAA); Flame Retardant - Glass Fiber - Low Warp
RTP Company RTP 205 G FR HS Nylon 4/6 (PA), Glass Fiber - Flame Retardant - Heat Stabilized - Dry As Molded
Lubrizol LifeSciences Carbopol® ULTREZ 10 NF Polymer
Lubrizol LifeSciences Carbopol® ETD 2020 NF Polymer
Lubrizol LifeSciences Carbopol® 980 NF Polymer

PLUBR8007 / 238955

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.