Tough, abrasion resistant polyester based urethane Key Properties: - Excellent physical properties
- Free of mercury, MOCA or TDI
- Antimicrobial / Antifungal
Applications: - Formulated for room temperature hand-batch or vacuum assisted processing
Cure 1: 7 days at 77°FInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |