MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Dow Engage® ENR 7467.00 Ethylene-Butene Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: ENR 7467.00 is a high performance ethylene-butene copolymer, offering superior impact properties for more demanding TPO applications. The polymer has very low crystallinity and is available as surface modified pellets for ease in handling and mixing.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.862 g/ccASTM D792
Viscosity 2.06e+6 cP
@Shear Rate 100 1/s,
Temperature 190 °C
100 rad/sec; ARES Rheometer
 4.20e+6 cP
@Shear Rate 10 1/s,
Temperature 190 °C
10 rad/sec; ARES Rheometer
 5.59e+6 cP
@Shear Rate 1.58 1/s,
Temperature 190 °C
1.58 rad/sec; ARES Rheometer
 6.58e+6 cP
@Shear Rate 0.1 1/s,
Temperature 190 °C
0.1 rad/sec; ARES Rheometer
Melt Index of Compound 1.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Crystallinity 5.4 %25°C; DuPont Test
 12.6 %
@Temperature -40.0 °C
Total; DuPont Test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 5610 sec; ASTM D2240
Tensile Strength, Ultimate 2.60 MPa508 mm/min; ASTM D638
Elongation at Break 760 %508 mm/min; ASTM D638
Flexural Modulus, 1% Secant 1145.8 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 36.0 °CDSC, 10°C/min (peak); DuPont Test
Crystallization Temperature 23.0 °CDSC, 10°C/min (peak); DuPont Test
Glass Transition Temp, Tg -56.0 °CDSC, 10°C/min (inf); DuPont Test
 
Descriptive Properties
Molecular Weight DistributionNarrowGPC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Engage® 8842 Polyolefin Elastomer
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer
Dow Engage® ENR 8556.00 Ethylene-Octene Copolymer
Dow Engage® 8180 Polyolefin Elastomer
Dow Engage® 8130 Polyolefin Elastomer

PDVE52 / 34113

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.