MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lord Adhesives 305 Epoxy Adhesive System
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD® 305 adhesive is a general purpose, medium viscosity, two-component epoxy adhesive system used for applications that require strong, durable, chemically and environmentally resistant bonds. This adhesive system provides excellent adhesion to prepared metals, fiberglass reinforced plastics (FRP), phenolic, wood, prepared rubber and other materials. It is also used to bond cured rubber to itself and rubber to metal, including gaskets, bushings, shock-absorbing devices and rubber rolls. LORD 305 adhesive can be either room temperature cured or heat cured for faster processing.

Features: provides load bearing properties equal to or greater than the materials being bonded. contains no solvent, nonflammable and virtually odorless. resists moisture, sunlight and weathering. performs at temperatures from -30°F to +250°F (-34°C to +121°C). resists dilute acids, alkalis, solvents, greases and oils. provides low shrinkage, good creep properties and low water absorption.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.929 - 1.00 g/cc0.0335 - 0.0361 lb/in³305-2 Hardener
 1.13 - 1.20 g/cc0.0407 - 0.0433 lb/in³305-1 Resin
Solids Content 100 %100 %mixed
Brookfield Viscosity  10000 - 18000 cP
@Temperature 25.0 °C
10000 - 18000 cP
@Temperature 77.0 °F
Brookfield HBF, Spindle 2, 10 rpm, 305-1 Resin
 20000 - 45000 cP
@Temperature 25.0 °C
20000 - 45000 cP
@Temperature 77.0 °F
Brookfield HBF, Spindle 2, 10 rpm, 305-2 Hardener
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.2 MPa2490 psiCured; ASTM D882-83A, modified
Elongation at Break 31 %31 %Cured; ASTM D 882-83A, modified
Modulus of Elasticity 5.16 GPa748 ksiCured; ASTM D882-83A, modified
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -34.4 °C-30.0 °F
Glass Transition Temp, Tg 61.0 °C142 °FCured; ASTM E1640-99, by DMA
Flash Point >= 93.0 °C>= 199 °FClosed Cup, 305-1 Resin
 >= 93.0 °C>= 199 °FClosed Cup, 305-2 Hardener
 
Processing PropertiesMetricEnglishComments
Pot Life 8.00 - 16.0 min8.00 - 16.0 minTime to Handling Strength, Mixed with hardener
Working Life 1.00 - 2.00 min
@Temperature 24.0 °C
1.00 - 2.00 min
@Temperature 75.2 °F
Mixed with hardener, 54 g mass
Shelf Life 24.0 Month
@Temperature 16.0 - 27.0 °C
24.0 Month
@Temperature 60.8 - 80.6 °F
from date of manufacture in original, unopened container, both components
 
Descriptive Properties
AppearanceBlue Liquid305-2 Hardener
 Clear Amber Liquid305-1 Resin
Cured AppearanceTranslucent Blue
Mixed AppearanceBlue Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9117 / 232505

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.