MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Zortrax Z-FLEX Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Z-FLEX is a thermoplastic polyester elastomer that can be 3D printed with at a relatively fast rate of 45mm/s. The filament has great interlayer adhesion and dimensional tolerance falling below +/- 0,02 mm. Z-FLEX is elastic, can bend without breaking, and is resistant to various chemicals including gasoline, ethyl alcohol, butane, and carbon monoxide. Compared to Z-SEMIFLEX, this filament is a little more elastic. Besides being able to withstand temperatures as high as 70° C, it can maintain its integrity in low temperatures reaching -40° C. Z-FLEX is perfect for 3D printing parts intended to be bent frequently like tires, elastic hinges, or gaskets.

Information provided by Zortrax

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.186 g/ccISO 1183-3:2003
Melt Flow 27.98 g/10 min
@Load 2.16 kg,
Temperature 225 °C
ISO 1133:2006
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 31ISO 868:1998
Tensile Strength at Break 9.07 MPaISO 527:1998
Tensile Strength 9.94 MPaISO 527:1998
Elongation at Break 3319.12 %ISO 527:1998
Elongation at Yield 3120.74 %ISO 527:1998
Flexural Strength 3.60 MPaISO 178:2011
Flexural Modulus 53.86 MPaISO 178:2011
Izod Impact, Notched (ISO) 14.61 kJ/m²ISO 180:2004
 
Thermal PropertiesOriginal ValueComments
Melting Point 174.25 °CISO 11357-3:2014

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZORT004 / 281883

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.