MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Hexcel® LC2000 Liquid Crystal Polymer for RF Interference Control
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Description:
  • Flame-retardant, rigid MAGRAM absorber capable of maintaining its structural integrity at elevated temperatures.
  • Designed for attenuation in the +1 GHz range.
  • Performance can be tailored to specific applications.
  • Designed to make rigid parts that will meet theUL-94 V-0 flammability requirements and standup over time to elevated temperatures.
  • Suited to be molded into a termination load, chip cap, or circuit cover.
  • Can be injection molded into custom parts of virtually any configuration.
  • Halogen free, RoHS and REACH compliant.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 90.090.0ASTM D2240
Tensile Strength 48.3 MPa7000 psiASTM D638
 55.8 MPa
@Treatment Temp. 105 °C,
Time 605000 sec
8100 psi
@Treatment Temp. 221 °F,
Time 168 hour
Thermal Aging; ASTM D638
Elongation at Break 2.00 %2.00 %ASTM D638
 2.00 %
@Treatment Temp. 105 °C
2.00 %
@Treatment Temp. 221 °F
Thermal Aging; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.10e+10 ohm>= 1.10e+10 ohmASTM D257
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9592 / 322746

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.