MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
American Elements Cerium Nanoparticles
Categories: Metal; Pure Element

Material Notes: General Description

Cerium (Ce) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Cerium Particles are typically 5 - 40 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 60 - 100 nm range with a specific surface area of approximately 5 - 10 m 2 /g. Nano Cerium Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Applications for cerium nanocrystals include numerous fuel cell functions such as in the electrolyte of solid oxide fuel cells (SOFC), to remove ultrafine diesel particle emissions like carbon and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications. Further research is being done for their potential electrical, dielectric, magnetic, optical, imaging, catalytic, biomedical and bioscience properties.

Key Words: Formula: Ce; CAS Number: 7440-45-1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.689 g/cc
Particle Size 0.0050 - 0.040 µm
 0.060 - 0.10 µm
Specific Surface Area 5.0 - 10 m²/g
 30 - 50 m²/g
Molecular Weight 140.12 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 795 °C
Boiling Point 3360 °C
 
Descriptive Properties
AppearanceBlack
StabilityEasily oxidized in the air

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EJAMER20 / 5503

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.