MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Cotronics Duralco™ 4703 Adhesive and Tooling Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: High temperature resin reinforced with ceramic and metallic fibers and particles, resulting in high thermal stability. Easily machined to close tolerances and will repair and rebuild worn or cracked composites, dies, fixtures, jigs, etc. Electrically non-conductive.

Corrosion Resistance: resistant to most chemicals, solvents, acids and bases.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/cc
Moisture Absorption at Equilibrium 0.15 %
Viscosity 50000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 95
Tensile Strength, Ultimate 11800 psi
Elongation at Break 2.0 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cm
Dielectric Strength 450 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 18.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 700 °F
Shrinkage 0.10 %
 
Processing PropertiesOriginal ValueComments
Cure Time 240 - 360 min
@Temperature 121 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cotronics Duralco™ 4525 Electrically Resistant, Room Temperature Curing Epoxy
Solvay CYCOM® 5276-1 Epoxy with G40-800 Tape Composite
Solvay FM® 680-1 Polyimide Film Adhesive
Abatron AboCast/AboCure 8501-5/8501-4 High Temperature Resistant Epoxy
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System

PCOTR0430 / 29068

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.