MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Zortrax Zortrax Resin Tough White/Grey
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Zortrax Resin Tough White/Grey is an ABS-like photopolymer resin with distinctive properties targeted at both professionals and hobbyists. It allows users to produce models with smooth surfaces and sharp details, which is crucial when assembling multiple items into one object. Thanks to the resin’s low shrinkage, separate elements of movable parts, functional prototypes, or action figurines match each other perfectly.

Applications: end-use products, functional prototypes, engineering prototypes, jigs and fixtures, elements of tools, products’ casing, artistic projects, action figurines/toys, movable parts.

Information provided by Zortrax

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.115 g/ccLiquid; ASTM D647-12
 1.211 g/ccSolid; ASTM D647-12
Viscosity 307 cPASTM D4212-10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86ASTM D2240-05
Tensile Strength 54.3 MPaASTM D790-10
Elongation at Break 13.9 %ASTM D638-14
Modulus of Elasticity 0.670 GPaASTM D638-14
Flexural Strength 63.8 MPaASTM D790-10
Flexural Modulus 1586.8 MPaASTM D790-10
Izod Impact, Notched (ISO) 58.1 kJ/m²ASTM D256-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZORT018 / 281897

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.