MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Danquinsa DANCURE® 101NV Isocyanate Hardeners
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCURE® 101NV is a water dispersible, aliphatic and low viscosity Polyisocyanate for the cross linking of adhesions on a aqueous basis of Polyurethane dispersions, acrylate dispersions and many other aqueous hydroxyl functional polymer dispersions. DANCURE® 101NV is an useful agent for the cross linking of aqueous lacquer and coating systems.

Application: DANCURE® 101NV is used as a cross linking agent for aqueous adhesives for aqueous lacquer films, paints and coatings. If DANCURE® 101NV is added, the improvement of the chemical-, temperature resistance as the adhesive force to several substrates will be much higher.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccDIN 51.757
Solids Content 79 - 91 %DIN 53.189
Brookfield Viscosity 100 - 300 cPRVT, spindle 4, at 20°C
Storage Temperature 10.0 - 30.0 °C
 
Thermal PropertiesOriginal ValueComments
Flash Point 170 °CDIN 51.755
 
Descriptive Properties
Aspecttransparent, clear low viscose liquid
Chemical compositionaliphatic Isocyanate, water dispersible
Composition<0.15%residual monomer content
 17.5-21.5%NCO- volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ106 / 294526

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.