MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco AREMCOLOX™ 502-900 CS-85 Calcium Silicate Machinable Ceramic, MGC
Categories: Ceramic; Machinable Ceramic; Oxide

Material Notes: Structural insulation that combines high strength and excellent thermal insulating characteristics for use in heat treating, fire protection, and electrical applications. Also ideal for direct contact with non-ferrous metals. Machines easily and is available in ¼” to 3” thick sheets × 4’ × 8’.

Vendors: Aremco offers a range of machinable ceramics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 20.7 MPa3000 psi
Compressive Strength 71.0 MPa10300 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.5e+12 ohm-cm4.5e+12 ohm-cmDC
Dielectric Strength 2.40 kV/mm61.0 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 982.2 °C1800 °FOxidizing
Maximum Service Temperature, Inert 1000 °C1830 °FInert
 1000 °C1830 °FVacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CAREM12e / 282875

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.