MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LEXAN FL2000 PC (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24" (6.0mm) wall. This product offers low temperature impact strength and high heat resistance in combination with LEXAN FL2000 resin is available in opaque colors only.

Information provided by SABIC Innovative Plastics for the Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccfoam molded; ASTM D 792
 1.21 g/ccASTM D 792
Water Absorption 0.13 %
@Time 86400 sec
ASTM D 570
Water Absorption at Saturation 0.34 %
@Temperature 23.0 °C
ASTM D 570
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
@Thickness 6.34 mm
SABIC Method
Melt Flow 10.3 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 53.0 MPa
@Thickness 6.35 mm
ASTM D 638
Elongation at Break 7.8 %
@Thickness 6.35 mm
ASTM D 638
Tensile Modulus 2300 MPa
@Thickness 6.40 mm
ASTM D 638
Flexural Yield Strength 75.0 MPa
@Thickness 6.40 mm
ASTM D 790
Flexural Modulus 1930 MPa
@Thickness 6.40 mm
ASTM D 790
Izod Impact, Unnotched 2670 J/m
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D 4812
Falling Dart Impact 122 J
@Temperature 23.0 °C
SABIC Method
Instrumented Impact Total Energy 8.00 J
@Temperature -40.0 °C
ASTM D 3763
 67.0 J
@Temperature -20.0 °C
ASTM D 3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.60e+16 ohm-cmASTM D 257
Surface Resistance >= 1.10e+17 ohmASTM D 257
Dielectric Constant 2.47
@Frequency 100 Hz
ASTM D 150
 2.68
@Frequency 1e+6 Hz
ASTM D 150
Dissipation Factor 0.0037
@Frequency 100 Hz
ASTM D 150
 0.0039
@Frequency 1e+6 Hz
ASTM D 150
Arc Resistance 60 - 120 secPLC 6; ASTM D 495
Comparative Tracking Index 100 - 175 VPLC 4; UL 746A
Hot Wire Ignition, HWI >= 120 secPLC 0; UL 746A
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minPLC 3; UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 55.8 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E 831
Specific Heat Capacity 1.18 J/g-°CASTM C 351
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
@Thickness 6.40 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
@Thickness 6.40 mm
unannealed; ASTM D 648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness 3.91 mm
UL 94
 V-1
@Thickness 5.99 mm
UL 94
Oxygen Index 28.2 %ASTM D 2863

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI46205 / 187290

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.