MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Osterman & Co Osterlene® LLH100-B LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LLH100 is a linear low density polyethylene grade for applications that require high strength and toughness. Typical applications include heavy duty shipping sacks, trash can liners, commercial and industrial packaging, as well as food and consumer packaging. This resin offers enhanced film strength, drawdown, toughness and heat seal strength. In addition this resin has excellent low temperature resistance for applications such as stretch film and frozen food packaging.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America
Additive: Additive: Antiblock: No; Slip: No
Features: Good Drawdown; Good heat Seal; High Strength; High Toughness; Low Temperature Resistance
Uses: Bags; Food Packaging; Heavy-duty Bags; Liners; Packaging
Processing Method: Extrusion

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 550 %ASTM D882
Film Elongation at Break, TD 750 %ASTM D882
Secant Modulus, MD 29.5 ksiASTM D790
Secant Modulus, TD 34.5 ksiASTM D790
Elmendorf Tear Strength MD 380 gASTM D1922
Elmendorf Tear Strength TD 700 gASTM D1922
Dart Drop Test 180 gF50; ASTM D1709
Film Tensile Strength at Break, MD 8500 psiASTM D882
Film Tensile Strength at Break, TD 6800 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 221 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 16 %ASTM D1003
Gloss 50 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POSTER108 / 267690

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.