MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials TIVAR® Cestigreen UHMW-PE Ultra High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: TIVAR® Cestigreen UHMW-PE is a permanently static dissipative material with extremely high molecular weight and has specifically been developed as an alternative for standard static dissipative UHMW-PE grades and more particularly for applications where a green and non-sloughing (without graphite or carbon powder) static dissipative UHMW-PE is required.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccISO 1183-1
Water Absorption <= 0.10 %
@Time 86400 sec
immersion in water; ISO 62
Water Absorption at Saturation <= 0.10 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ISO 868
Tensile Strength 20.0 MPaISO 527-1/-2
Elongation at Break >= 50 %ISO 527-1/-2
Elongation at Yield 15 %ISO 527-1/-2
Modulus of Elasticity 0.770 GPaISO 527-1/-2
Compressive Strength 7.00 MPa
@Strain 1 %
ISO 604
 11.0 MPa
@Strain 2 %
ISO 604
 17.5 MPa
@Strain 5.0 %
ISO 604
K Factor (ISO) 6.0 µm/kmISO 7148-2
Charpy Impact Unnotched NBISO 179-1/1eU
Charpy Impact, Notched 60.0 kJ/m²ISO 179-1/1eA
 70.0 kJ/m²double 14° notched; ISO 11542-2
Coefficient of Friction, Dynamic 0.15 - 0.30QTM 55007
Limiting Pressure Velocity 0.0500 MPa-m/sec1 m/s cylindrical sleeve bearings
 0.0800 MPa-m/secat 0.1 m/s cylindrical sleeve bearings
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.400 W/m-K
Melting Point 135 °C10°C / min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C20,000 hours
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °CISO 75-1/-2
Minimum Service Temperature, Air -150 °C
Flammability, UL94 HB
@Thickness 3.00 mm
Oxygen Index <= 20 %ISO 4589-1/-2
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM916 / 291073

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.