MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Radici Radistrong ® A RV500W 333 BK Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Special PA 50% glass fiber reinforced, injection molding grade. Heat stabilized. Black color.

Product with enhanced mechanical properties, suitable for demanding applications as in case of metal replacement.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccISO 1183
Water Absorption 3.8 %
@Thickness 2.00 mm,
Time 86400 sec
Immersion @ 23°C; ISO 62
Moisture Absorption 0.900 %
@Thickness 2.00 mm,
Temperature 23.0 °C
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 190 MPa5mm / min. Conditioned; ISO 527-2/1A
 250 MPa5mm / min. DAM; ISO 527-2/1A
Elongation at Break 2.3 %5 mm / min. DAM; ISO 527-2/1A
 3.0 %5 mm / min. Conditioned; ISO 527-2/1A
Tensile Modulus 14600 MPa1mm / min. Conditioned; ISO 527-2/1A
 17600 MPa1mm / min. DAM; ISO 527-2/1A
Flexural Strength 300 MPa2mm / min. Conditioned; ISO 178
 375 MPa2mm / min. DAM; ISO 178
Flexural Modulus 15400 MPa2mm / min. Conditioned; ISO 178
 16300 MPa2mm / min. DAM; ISO 178
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 81.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 95.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 102 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 1.70 J/cm²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohmDAM; 500V.; IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 17.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 258 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 245 °CISO 75/2Af
Flammability, UL94 HB.8
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °CInjection Molding
Mold Temperature 90.0 - 120 °C
 
Descriptive Properties
Injection Molding Injection SpeedMedium - high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6969 / 293474

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.