MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® 680 High Strength/High Viscosity Retaining Compound
Categories: Polymer; Adhesive; Thermoset

Material Notes:
Retainers
Loctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. Finding wide acceptance as a standard method for assembling press and slip-fitted parts, Loctite® Retaining Compounds fill the "inner space" between components and cure to form a strong precision assembly. Formulated in a selection of viscosities, gap filling ability, flexibility and strength characteristics, Loctite® Retaining Compounds can be applied with automatic process equipment or dispensed manually.

Loctite® 680 High Strength/High Viscosity Retaining Compound
A retaining compound for joining fitted cylindrical parts. Fixtures in 10 minutes and provides a shear strength of 4,000 psi on steel after 24 hours. Fills diameter gap distances up to 0.015".
Recommended Primer: 7471 (T).
NSF/ANSI 61 approved
Typical Use: High strength for slip fitted parts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/cc
Viscosity 1250 cP
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 4000 psiSteel/Steel; Varies with substrates
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -65.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
 24.0 hour
@Temperature 25.0 °C
Full Cure; Steel
 
Descriptive Properties
ColorGreen
Gap Fill0.015 in.Diametral

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Granite
Raschig Group PiMC 1949 Granite colors
Verde Fuoco Metasomatite Architectural Stone
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)
Schott BOROFLOAT® Borosilicate Float Glass

PLOCT127 / 51863

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.