MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® AT-1125 HS PPA, 25% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: 25% glass fiber, impact modified, heat stabilized

Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stability, chemical resistance and ductility. This resin has a high heat deflection temperature and a high flexural modulus, with greater tensile elongation than untoughened glass-reinforced PPA.

Typical applications include bearings, bearing retainers/cages, housings, chemical processing equipment components, motor frames, sporting equipment, lawn and garden equipment and components that require press-fit or snap-fit assembly.

- Black: AT-1125 HS BK 324

Markets/Uses: Automotive / Fuel Systems / Fuel Sender Units; Miscellaneous / Consumer Goods / Appliances; Plumbing / Mechanical Parts / Structural Parts

Applications: Appliance Components; Appliances; Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bearings; Connectors; Fuel Lines; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement

Features: Chemical Resistant; Good Dimensional Stability; Heat Stabilized; High Heat Resistance; Impact Modified

Injection notes: Storage: - Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccMethod A; ISO 1183
Water Absorption 0.20 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 174 MPaASTM D638
 190 MPaISO 527-2
Elongation at Break 2.5 %ISO 527-2
 3.2 %ASTM D638
Tensile Modulus 8480 MPaASTM D638
 8890 MPaISO 527-2
Flexural Strength 240 MPaISO 178
Flexural Yield Strength 255 MPaASTM D790
Flexural Modulus 7580 MPaASTM D790
 7790 MPaISO 178
Izod Impact, Notched 120 J/mASTM D256
Izod Impact, Unnotched 1100 J/mASTM D256
Izod Impact, Notched (ISO) 8.80 kJ/m²Type 1, Notch A; ISO 180
Charpy Impact, Notched 8.80 kJ/m²Type 1, Edgewise, Notch A; ISO 179
Dart Drop, Total Energy 2.03 JInstrumented Dart Impact, Energy as Maximum Load; ASTM D3763
 13.8 JInstrumented Dart Impact; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Melting Point 311 °CPeak; ASTM D3418
 311 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 279 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 235 °CUnannealed; ASTM D648
 280 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Feed Temperature 79.0 °CInjection Hopper
Rear Barrel Temperature 304 - 318 °C
Front Barrel Temperature 316 - 329 °C
Melt Temperature 321 - 343 °CInjection
Mold Temperature 135 °C
Drying Temperature 121 °C
@Time 14400 sec
Moisture Content 0.030 - 0.060 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer; Impact Modifier
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4103 / 279903

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.