33% glass fiber, for thick-wall parts (>3mm), fast cycle time, hot-water molds, heat stabilized, lubricated Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samples dry as molded and samples conditioned to 50% relative humidity in accordance with ISO-1110, Accelerated Method. Typical applications include electrical and electronic components especially for automotive systems. - Black: AS-4133 HS BK 324 - Natural: AS-4133 HS NT Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Cell Phones; Connectors; Electrical/Electronic Applications; General Purpose; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Thick-walled Parts; Valves/Valve Parts Features: Chemical Resistant; Creep Resistant; Fast Molding Cycle; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Hot Water Moldability; Laser Weldable; Low Moisture Absorption; Lubricated Injection notes: Injection Rate: 3 to 4 in/sec Holding Pressure: 50% of injection pressure Storage: - Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide. Information provided by Solvay Specialty Polymers. |