MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Chockfast® PHILLYBOND #6 Epoxy Paste
Categories: Polymer; Thermoset; Epoxy

Material Notes: PHILLYBOND #6 is a two-component, high strength epoxy paste for the repair of punctures or cracks in tanks, pumps, pipes, steam lines, sea chests, valve bodies, etc. The material is also used to fill holes, voids and to provide a smooth surface for repairs [at temperatures up to 428°F (220°C)], PHILLYBOND #6 is resistant to most acids, alkali and hydrocarbons and will adhere to clean surfaces such as steel, cast iron, bronze, aluminum, copper, nickel, wood and most plastics.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 1000 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 428 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 22.0 °C
@ 1/2inch thickness
Pot Life 10.0 - 15.0 min
@Temperature 22.2 °C
Shelf Life 24.0 MonthIf stored in a cool, dry area.
 
Descriptive Properties
Colorblackhardener
 graymixed
 whiteresin
Mix Ratio by volume4 to 1
Mix Ratio by weight4 to 1
Viscositypaste/putty

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWC9030 / 239540

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.