MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® ABLESTIK 84-1LMISNB Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Silver

Product Benefits:

  • Electrically conductive
  • High purity
Cure: Heat cure

Application: Die attach

Filler Type: Silver

LOCTITE ABLESTIK 84-1LMISNB adhesive is designed for semiconductor packaging applications.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 14000 cPUncured, Speed 10 rpm
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 250 MPa
@Temperature 250 °C
Cured
 450 MPa
@Temperature 150 °C
Cured
 5000 MPa
@Temperature 25.0 °C
Cured
 6100 MPa
@Temperature -65.0 °C
Cured
Shear Strength 8.28 MPa
@Temperature 200 °C
Lap
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.00020 ohm-cmCured
 
Thermal PropertiesOriginal ValueComments
CTE, linear 54.0 µm/m-°CCured, Below Tg
 190 µm/m-°CCured, Above Tg
Thermal Conductivity 3.50 W/m-KCured
Glass Transition Temp, Tg 115 °CCured, TMA
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 200 °C
Alternate Cure Schedule
Working Life 168 hour
Shelf Life 12.0 Month
@Temperature -40.0 °C
Uncured, from date of manufacture
 
Descriptive Properties
Extractable Ionic Content (ppm)<10Cured, Chloride (Cl-)
 <10Cured, Potassium (K+)
 <20Cured, Sodium (Na+)
Shear Strength12 kg-f/die2 X 2 mm (80 x 80 mil) Si die on Ag/Cu LF
Water Extract Conductivity8 µmhos/cmCured
Weight Loss (%)0.45Cured @ 300ºC, TGA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5004 / 255215

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.