1527 White, also called 1527SWT is a white, UL certificated, one component RTV silicone with super resistance to weathering and ultra violet(UV). This material has very good adhesion without the need for primers to a wide range of substrates. It can be used for a variety of interior and exterior bonding and sealing applications. 1527 White is formulated to perform at temperatures ranging from -54°C to 210°C. Features and Benefits: - Excellent heat resistance properties
- Super resistance to ultra violet(UV) and weather
- Neutral cure low/no odor
- UL Certified
- Wide operating temperature range
- Easy to use for reworkable applications
Information provided by H.B. Fuller Company |